Nylon 6 vs. Nylon 66 - Leitfaden zur Auswahl technischer Kunststoffe

nylon 6 plastic pellets granules industrial packaging
Nylon 6 vs. Nylon 66 - Leitfaden zur Auswahl technischer Kunststoffe
Nylon 6 vs. Nylon 66 - Leitfaden zur Auswahl technischer Kunststoffe
Nylon 6 vs. Nylon 66 - Leitfaden zur Auswahl technischer Kunststoffe
Nylon 6 vs. Nylon 66 - Leitfaden zur Auswahl technischer Kunststoffe
Nylon 6 vs. Nylon 66 - Leitfaden zur Auswahl technischer Kunststoffe
Nylon 6 vs. Nylon 66 - Leitfaden zur Auswahl technischer Kunststoffe
Nylon 6 vs. Nylon 66 - Leitfaden zur Auswahl technischer Kunststoffe

Chemical Structure Differences

The fundamental difference between PA6 (Nylon 6) und PA66 (Nylon 66) lies in their molecular structure:

  • Nylon 6: Made from caprolactam, has 6 carbon atoms in each repeating unit. Less crystalline structure.
  • Nylon 66: Made from hexamethylenediamine and adipic acid, has two 6-carbon chains. More crystalline structure.

Mechanical Properties Comparison

Eigentum PA6 PA66
Zugfestigkeit 70-85 MPa 80-100 MPa
Biegemodus 2.5-3.0 GPa 2.8-3.5 GPa
Dehnung beim Bruch 30-100% 15-60%
Izod-Schlagzähigkeit mit Kerbe 50-100 J/m 40-80 J/m
Schmelzpunkt 220 °C 260 °C
HDT at 1.8 MPa 70°C 90°C

Feuchtigkeitsabsorption

Moisture absorption is critical for nylon applications:

Zustand PA6 PA66
At 50% RH 2.5-3.0% 2.0-2.5%
Sättigung 8-10% 6-8%

Processing Characteristics

Nylon 6 Processing

  • Melting Point: 220 °C
  • Processing Range: 240-280°C
  • Temperatur der Form: 40-80°C

Nylon 66 Processing

  • Melting Point: 260 °C
  • Processing Range: 280-320°C
  • Temperatur der Form: 60-90°C

Applications by Material

Nylon 6 Applications

  • Gears and sprockets
  • Industrial monofilament
  • Film and packaging
  • Consumer products

Nylon 66 Applications

  • Automotive under-hood components
  • Electrical connectors
  • High-temperature bearings
  • Precision mechanical components

Reinforced Grades

Both materials are commonly reinforced with glass fiber:

Klasse PA6 + GF30 PA66 + GF30
Zugfestigkeit 140-160 MPa 170-200 MPa
HDT (1.8 MPa) 205°C+ 250°C+
Feuchtigkeitsabsorption 1.0-1.5% 0.8-1.2%

Selection Summary

Choose Nylon 6 when:

  • Impact resistance is critical
  • Cost sensitivity is high
  • Operating temperatures are moderate

Choose Nylon 66 when:

  • Higher mechanical strength is required
  • Elevated temperatures are expected
  • Dimensional stability is critical

FAQ

When is Nylon 6 vs Nylon 66 — Engineering Plastic Selection Guide a good option?

Nylon 6 vs Nylon 66 — Engineering Plastic Selection Guide is a good option when fast iteration, complex geometry, low tooling cost, or low-volume production is more important than molded-part unit cost.

What should be checked before choosing Nylon 6 vs Nylon 66 — Engineering Plastic Selection Guide?

Prüfen Sie die Größe des Teils, die Materialeigenschaften, die Oberflächenbeschaffenheit, die Maßtoleranz, die Wärmeeinwirkung, die Belastungsrichtung und ob eine Nachbearbeitung erforderlich ist.

How does Nylon 6 vs Nylon 66 — Engineering Plastic Selection Guide compare with CNC machining?

Mit dem 3D-Druck lassen sich komplexe Formen schnell erstellen, während die CNC-Bearbeitung für präzise Oberflächen, engere Toleranzen und serienreife Materialien oft besser geeignet ist.

What affects the cost of Nylon 6 vs Nylon 66 — Engineering Plastic Selection Guide?

Die Kosten hängen vom Material, dem Bauvolumen, der Druckzeit, der Schichthöhe, der Entfernung von Stützen, der Endbearbeitung, der Prüfung und der Anzahl der Teile im Bau ab.

Entwerfen wir Ihre individuelle Lösung

Dieses Feld ist erforderlich.
Dieses Feld ist erforderlich.
Dieses Feld ist erforderlich.
Dieses Feld ist erforderlich.
Dieses Feld ist erforderlich.

Weiterführende Lektüre

Nach oben blättern