Why Lubricate Nylon?
Nylon’s natural surface properties include a relatively low coefficient of friction compared to many engineering plastics—but it’s not inherently self-lubricating. In moving-part applications like gears, bearings, slides, and cams, unlubricated nylon can experience accelerated wear, frictional heating, and stick-slip behavior. Lubricated nylon grades solve this by incorporating solid or liquid lubricants directly into the polymer matrix, creating parts that run smoothly for millions of cycles without external lubrication.
The lubricant additives work by forming a transfer film on the mating surface. As the nylon part moves, microscopic lubricant particles are released, coating both the nylon surface and the opposing metal or plastic surface. This film reduces the coefficient of friction from 0.35–0.40 (unmodified nylon on steel) down to 0.10–0.20, depending on the lubricant type and loading.
The Three Main Lubricant Types
| Lubricant | Typical Loading | COF (vs Steel) | Beste Bewerbung |
|---|---|---|---|
| PTFE (Teflon) | 10–20% | 0.10–0.18 | High-speed bearings, low-load slides |
| MoS₂ (Molybdenum Disulfide) | 1–5% | 0.12–0.20 | High-load gears, thrust washers |
| Oil-filled | 2–8% | 0.08–0.15 | Precision bearings, low-noise applications |
PTFE-Filled Nylon
PTFE (polytetrafluoroethylene) is the most common solid lubricant for nylon. With a coefficient of friction as low as 0.04 in its pure form, PTFE particles dispersed throughout nylon create an extremely low-friction surface. PTFE-filled nylons are ideal for high-speed, low-to-moderate load applications where continuous sliding motion is required.
The limitation: PTFE reduces mechanical strength by 10–20% and increases cost. It also doesn’t perform as well as MoS₂ under very high contact pressures.
MoS₂-Filled Nylon
Molybdenum disulfide has a layered crystal structure similar to graphite—sheets that easily slide past each other. This makes it exceptional under high contact pressures where PTFE would be squeezed out. MoS₂-filled nylon is the go-to choice for gears, cams, and thrust washers operating under significant load.
MoS₂ also increases nylon’s crystallinity slightly, which can improve strength and stiffness—unlike PTFE which weakens the matrix. The dark gray/black color can be a consideration for visible parts.
Oil-Filled Nylon
Oil-filled nylons incorporate lubricating oil directly into the polymer during compounding. During operation, the oil slowly migrates to the surface, providing continuous lubrication throughout the part’s life. This “self-replenishing” characteristic makes oil-filled nylon excellent for sealed applications where relubrication is impossible.
Common oils include silicone, mineral oil, and synthetic hydrocarbon oils. The oil content is precisely controlled to avoid excessive migration that could contaminate surrounding components.


Wear Rate Comparison
| Nylon-Sorte | K-Factor (×10⁻⁸ mm³/N·m) | PV Limit (MPa·m/s) | Service Temp Range |
|---|---|---|---|
| PA6, ungefüllt | 40–80 | 0.09–0.12 | -30°C to 85°C |
| PA6 + 15% PTFE | 5–12 | 0.15–0.25 | -40°C to 100°C |
| PA6 + MoS₂ | 8–15 | 0.20–0.35 | -30°C to 95°C |
| PA66 + Aramid + PTFE | 2–5 | 0.35–0.50 | -40°C to 120°C |
Design Guidelines for Lubricated Nylon Parts
- Surface finish of the mating part: Aim for 0.2–0.4 μm Ra on the steel/opposing surface. Rougher surfaces accelerate wear.
- Clearance: Allow 0.3–0.5% of the bearing diameter for thermal expansion and water absorption swell.
- Wandstärke: Maintain uniform wall thickness to avoid warpage that creates uneven wear patterns.
- Running-in period: Expect higher friction during the first 500–1000 cycles as the transfer film establishes.
- Combination with glass fiber: Adding glass fiber to lubricated nylon improves load capacity but increases wear on the mating surface. Use hardened steel (58+ HRC) for mating parts.
Warum sollten Sie Nylon-Kunststoff für Ihren Bedarf an technischen Kunststoffen wählen?
- ✅ 300+ Spritzgießmaschinen von 50T bis 2000T
- ✅ Mehr als 10.000 Teile pro Tag Produktionskapazität
- ✅ ±0,02mm Genauigkeit Toleranz für alle Materialien
- ✅ MOQ nur 1 Stück für das Prototyping; skalierbar auf Millionen
- ✅ 24-Stunden-Quotierung, 3-15 Tage Vorlaufzeit
- ✅ ISO 9001 zertifiziertes Qualitätsmanagementsystem
Verwandte Artikel
- Nylon vs. POM (Acetal/Delrin): Die Wahl zwischen zwei technischen Kunststoffen
- Materialeigenschaften von Nylon: Eine vollständige technische Referenz
- Long Glass Fiber vs Short Glass Fiber Reinforced Nylon
FAQ
How do you know whether Lubricated Nylon Grades: PTFE, MoS₂ and Oil-Filled Options for Wear Applications fits a part?
Lubricated Nylon Grades: PTFE, MoS₂ and Oil-Filled Options for Wear Applications fits a part when its load capacity, temperature range, moisture exposure, wear behavior, and processing method match the real service conditions.
What properties should be checked for Lubricated Nylon Grades: PTFE, MoS₂ and Oil-Filled Options for Wear Applications?
Prüfen Sie Festigkeit, Steifigkeit, Schlagfestigkeit, Hitzebeständigkeit, Feuchtigkeitsaufnahme, Formstabilität, Reibung, Verschleiß und chemische Verträglichkeit.
What is the biggest selection risk for Lubricated Nylon Grades: PTFE, MoS₂ and Oil-Filled Options for Wear Applications?
Das größte Risiko besteht darin, sich auf einen Wert aus dem Datenblatt zu verlassen, ohne die tatsächlichen Umgebungsbedingungen, das Verarbeitungsverfahren, die Bauteilgeometrie und die langfristige Nutzung zu berücksichtigen.
When should Lubricated Nylon Grades: PTFE, MoS₂ and Oil-Filled Options for Wear Applications be tested before production?
Prüfungen werden empfohlen, wenn das Bauteil Belastungen, Hitze, Chemikalien, Feuchtigkeit, engen Toleranzen, gesetzlichen Anforderungen oder einer neuen Betriebsumgebung ausgesetzt ist.