PA66 GF10 Glass Fiber Reinforced Nylon 66 Pellets

PA66 GF10 is nylon 66 reinforced with 10% glass fiber, supplied as pellets for injection molding. It is a lightly reinforced option for small housings, fan blades, gears and precision molded structures.

Material: 10% glass-fiber-reinforced nylon 66 pellets.

Reference grade: PA66 WHG10A, as named in the supplier PDF; typical tensile strength 110 MPa.

Anwendungen: Small housings, fan blades, gears, brackets and appliance supports.

Selection: Provide dimensions, load, service conditions, color and quantity.

Kategorien: ,

PA66 GF10 Material Overview

PA66 GF10 is nylon 66 reinforced with 10% glass fiber, supplied as pellets for injection molding. It is a lightly reinforced option for small housings, fan blades, gears and precision molded structures.

Artikel Einzelheiten
Polymer PA66 (nylon 66)
Verstärkung 10% glass fiber
Formular Pellets
Reference grade PA66 WHG10A
Verarbeitung Spritzguss

Typical Material Properties

Reference grade: PA66 WHG10A. The following values are from the supplier datasheet linked below; they are typical material values, not finished-part specifications.

Eigenschaft Typischer Wert Einheit Prüfverfahren
Zugfestigkeit 110 MPa ISO 527-2
Zugdehnung bei Bruch 13 % ISO 527-2
Biegemodul 3840 MPa ISO 178
HDT, Methode B 185 °C ISO 75-2/B
Dichte 1.19 g/cm³ ISO 1183
Formschrumpfung 0.7 % ISO 2577

HDT is reported under method B. The source does not state specimen conditioning. Confirm the current grade and test conditions before design approval.

Download PA66 WHG10A supplier datasheet (PDF)

PA66 GF10 Applications

Nine illustrative PA66 GF10 application and development examples; see the descriptions below
Illustrative applications; confirm the selected grade for your part. Tap the image to enlarge.

Sensor housings and connector housings.

Small housings need accurate fit, stable pin locations and sound weld lines. Confirm fluid exposure and any electrical requirements for the selected formulation.

Cooling-fan blades and small gears.

Review the rotating load, wear surfaces, operating temperature and assembly fit. Validate noise, vibration and dimensions with molded parts.

Brackets, cable-carrier links and appliance supports.

Ribs, hinge points and screw bosses need enough toughness as well as stiffness. Check repeated loading and fit after the part has reached its expected moisture condition.

Processing and Part Checks

Use the selected grade’s drying and molding instructions. Check gate position, fiber orientation, weld lines, shrinkage and critical dimensions during trials. Confirm performance on parts made with the intended tool and process.

For finished components, continue to Spritzgießen. For a material comparison, use the engineering plastics range.

Material Supply and Manufacturing Support

Nylon Kunststoff connects engineering plastic supply with custom manufacturing. WANHAN is our cooperating compounding factory; the photographs below show its material-feeding equipment, extrusion process and laboratory.

Material feeding equipment at WANHAN, Nylon Plastic’s cooperating factory
Material feeding
Extruded plastic strands at the WANHAN cooperating factory
Extrusion process
Laboratory work area at the WANHAN cooperating factory
Laboratory

Grade and formulation selection

Share your current grade, application and operating conditions. We coordinate the material review and identify the matching datasheet for the formulation offered.

Quality documents for your order

Specify the TDS, batch records, inspection requirements or compliance files your purchasing team needs. The documents and acceptance criteria are agreed for the quoted material.

Support beyond resin pellets

For a finished component, connect material selection with part design, tooling and molding review. Start with the drawing, expected quantity and critical dimensions.

Cooperating Factory Management-System Certificates

The supplied ISO 9001, ISO 14001 and ISO 45001 certificates identify Guangdong Wanhan as the certified entity. Their scope concerns modified plastic granules and the related management activities; it does not certify every material grade or every finished-part manufacturing service.

Review manufacturing capabilities and quality documentation. For document approval, match the legal entity, certificate scope and quoted grade.

PA66 GF10 — Frequently Asked Questions

What is PA66 GF10 supplied as?

It is nylon 66 with 10% glass fiber, supplied as pellets for molding. The linked supplier datasheet identifies the reference grade as PA66 WHG10A.

Where is PA66 GF10 used?

Application candidates include sensor housings, connector shells, small gears, cooling-fan parts, cable-carrier links and appliance supports. Check stiffness, toughness and dimensional requirements against the actual component.

Can I replace a higher glass-fiber grade with PA66 GF10?

Do not treat different reinforcement levels as interchangeable. Compare the exact grades’ mechanical and thermal data, then check the drawing, loads and molded-part performance before changing material.

What molding checks matter for PA66 GF10?

Confirm drying and molding instructions for the quoted grade. Review gate and weld-line locations, moisture conditioning and critical dimensions during sample trials.

Is PA66 GF10 automatically approved for electrical or medical use?

No. The material name and glass content do not establish a flame rating, electrical approval or medical qualification. State the applicable standard and required documents when requesting a formulation.

What should I send for PA66 GF10 selection and pricing?

Send the part application, present material if known, service temperature, color, quantity and destination. Include drawings and required qualification records when the inquiry covers finished components.

Request Material Data and a Quote

Send the application, current material if available, service temperature, load or fluid exposure, color, expected quantity and delivery destination. Add a drawing when finished parts are needed.

Request PA66 GF10 TDS and Quote

Nach oben blättern

Kontakt aufnehmen

Füllen Sie das nachstehende Formular aus, und wir werden uns in Kürze mit Ihnen in Verbindung setzen.

Kontaktinformationen